鎢表格可

鎢絲, 鎢杆, 鎢棒, 鎢條, 鎢箔, 鎢板, 鎢板, 鎢粉, 鎢管, 鎢坯, 鎢半成品和自訂完成鎢零件.

加工鎢

Tungsten can be very difficult to fabricate because of its high hardness and low ductility. Tungsten is a strong, 硬, 是通常在室溫脆性的裂紋敏感金屬. It requires special handling and skill beyond that necessary for most metals and alloys. It is important to remember when working with Tungsten is that it must be cut or formed at temperatures well above its transition temperature. Failure to do this may result in cracking or lamination. Care should be taken to insure that the metal remains at this temperature throughout the entire forming process. The use of cold tooling which rapidly chills the metal can be as harmful as not preheating the material. The best method for machining that involves metal removal is E.D.M. The following conventional methods can also be used with great care: 磨削, 形成, 加入, 銑削, 鉚接, 紡紗, 衝壓, 和車削.

車削
工具Carbide H(2)
Clearance angle
背耙子27°
側耙子
切削速度132 ft per minute
Nose Angle90°
刀尖圓弧半徑
磨削 (Use aluminum oxide or silicon carbide wheels with medium hardness.)
Wheel Typesilicon carbide; hardness j to l ; gram size 100-120
Speed12 ft per second
銑削 (When milling Tungsten, the following is recommended)
Cutting speed73 每分鐘英尺
clearance angle
side rake10°
形成 (When spinning, bending or stamping note the following)
模具Carbide
Temperature1000° – 1500° F

要求報價